A Happy Customer
Author: Mike Deakin, Pellets, LLC
Source: The Shot Peener magazine, Vol 33, Issue 3, Summer 2019
Doc ID: 2019031
Year of Publication: 2019
Abstract:
Following a two-year study, a major
automotive parts manufacturer converted their
multiple shot peening machines, one at a time,
from cast steel peening shot to Pellets stainless
steel (302/304 alloy) conditioned cut wire shot.
After several months of using the stainless steel
cut wire shot, the customer reported positive
results to the Pellets’ staff.