Cut Wire or Cast Steel Shot – A Review
Author: Kumar Balan
Source: The Shot Peener magazine, Vol 34, Issue 1, Winter 2020
Doc ID: 2020005
Year of Publication: 2020
Abstract:
INTRODUCTION
One of the challenges in our industry has been to increase the
awareness for shot peening, but with concerted efforts we are
seeing this move in a positive direction. During a re-cap after
the recent EI USA Shot Peening Workshop, the instructors
all agreed that the understanding and participation level of
students had increased over the years. The questions and
comments discussed in the classes were quite advanced. That
said, I would like to highlight a recurring conversation at the
workshop that will benefit from additional elaboration. This
discussion pertains to the choice between conditioned cut
wire (CW) shot and cast steel shot.