PRESS RELEASE: WA CLEAN Technology Receives ISO Certification
Author: Claudiu Ionescu, Stelux Manager & Customer Solutions Engineer, Winoa
Source: The Shot Peener magazine, Vol 34, Issue 1, Winter 2020
Doc ID: 2020010
Year of Publication: 2020
Abstract:
The WA CLEAN Technology is an electronic
optical device using as its working principle the analytical
colorimetry to support the visual assessment of the surface
preparation grades of uncoated steel substrates as defined in
ISO 8501-1 or in SSPC-VIS 1. In July 2019, the WA CLEAN
Technology received official accreditation via the ISO/TR
22770.
WA CLEAN Technology Adopted by the End Users
WA CLEAN Technology has been adopted in several
industrial fields and not only in surface preparation projects.
The WA CLEAN device has been developed in order to
help our customers to implement the ISO 8501-1 standard.
To avoid any misinterpretation, the goal of the device is not
to replace the ISO 8501-1, but to support the appropriate
implementation.