The Effect of Fine Particle Shot Peening on Carburized Material
Author: Yuji KOBAYASHI
Source: The Shot Peener magazine, Vol 35, Issue 2, Spring 2021
Doc ID: 2021015
Year of Publication: 2021
Abstract:
1. INTRODUCTION Shot peening is a process that improves the near-surface
properties of metals by impacting the metal surface with small
balls called shot that are made of metal or ceramic materials.
The main effect is to improve the fatigue strength and it is
used for various automotive parts.
The dent is created at the surface due to impact by shot
during the shot peening process. The surface roughness
characteristics will be modified by the peening process.
Changes to the surface are dependent on shot peening
conditions and the mechanical properties of metal parts.
| Download PDF |
|---|