Shot Peening and the Dynamic Root Strength of Gears
Author: Darko MalnariÄ, FerroECOBlast® Europe
Source: The Shot Peener magazine, Vol 35, Issue 3, Summer 2021
Doc ID: 2021027
Year of Publication: 2021
Abstract:
WITH MORE than 55 years of experience, FerroECOBlast®
Europe, based in Dolenjske Toplice, Slovenia, is one of the
global leaders in the field of surface treatment technologies.
What makes us stand out from the crowd is our dedication to
research and development. The following study, performed
by our R&D department, in collaboration with the IMT—
The
Institute of Metals and Technology from Slovenia—explores
the effect of shot peening on the dynamic root strength of
gears treated with different parameters in different heat
treatment methods.