The 2021 Workshop
Author: Jack Champaigne, Editor
Source: The Shot Peener magazine, Vol 36, Issue 1, Winter 2022
Doc ID: 2022001
Year of Publication: 2022
Abstract:
THE 29TH Electronics Inc. Shot Peening and Blast Cleaning Workshop and Trade Show was a success. I think everyone was happy to return to this level of normalcy in our industry.
One of my favorite aspects of this year’s event was the new technology at the trade show, in the classroom, classroom, and even in our photography.
| Download PDF |
|---|