Evolution of the controlled shot peening process in the automotive field

Author:  E. Morgano SILCO - Rivalta TO
Source:  ICSP14 Milan
Doc ID:  2022105
Year of Publication:  2022
Abstract:  
Introduction The controlled shot peening process, on a mechanical component, represents the most robust solution to increase its resistance to fatigue; moreover, since it is usually the last operation in the production chain, it does not change the parameters of the previous operations, such as forging, mechanical processing and surface hardening treatments.