Patents Relating to Shot Peening

The articles below are archived in the shotpeener.com Library. You can search these articles by using the keyword search below. Click on an article title to view details and access a free full text pdf. Search Tips

Total articles (550)

Page 19 of 40

  • Double Peening - (an explaination of U.S. Patent 3,073,022)
  • Year: 1988, Source: US Patent 3,073,022
  • This patent relates to first shot peening in a conventional manner and then applying a second treatment which differs from the first operation....

  • Preventing Stress Corrosion Cracking of Bearings
  • Year: 1987, Source: US Patent 4,687,556
  • A method of inhibiting stress corrosion cracking of a bearing of the type installed on a shaft with an interference fit. The surface of the inner ring is shot peened at least at and near the junctures...

  • Method for Making Spherical Particles
  • Year: 1987, Source: US Patent 4,643,753
  • A process and apparatus for spheridizing irregularly shaped minute particles, and the spheres produced thereby, in which a thin carbonaceous coating is applied to the particles in a unique manner, and...

  • Hose Coupling
  • Year: 1987, Source: US Patent 4,658,326
  • The present invention relates to a high impact hose coupling having a hollow body constructed of plastic, a helical restriction means to hold the hose end within the coupling body, a double locking me...

  • Method of Forming a Fine Grain Structure on the Surface of an Aluminium Alloy
  • Year: 1987, Source: US Patent 4,799,974
  • An aluminium alloy is provided which has a surface with a fine grain structure. It is produced by overaging an aluminium alloy and then cold working only the surface by shot peening or other surface w...

  • Installation for the Detensioning of Expanded Tubes, Particularly in a Heat Exchanger
  • Year: 1987, Source: US Patent 4,821,545
  • Detensioning of expanded tubes is brought by way of an installation using a rotopeening method. The tool is constituted by a cage moved along a helical path centered on the axis of the tube to be trea...

  • Portable Abrasive Blasting Gun Assembly
  • Year: 1987, Source: US Patent 4,674,239
  • Am improved protable abrasive blasting gun assembly which comprises a gun part having a compressed air conduit and an abrasive material conduit intersecting with one another to produce an abrasive car...

  • Rotopeening Apparatus Having a Flexible Spindle
  • Year: 1986, Source: US Patent 4,616,496
  • A rotopeening apparatus utilizing a flexible spindle for rotopeening the inside wall of tubes of limited access is disclosed herein. The spindle is formed from a flexible, rotatable housing and includ...

  • Method for Improving the Release and Finish Characteristics of Metal Stamping Dies
  • Year: 1986, Source: US Patent 4,581,913
  • A method for improving the release and finish characteristics of metal stamping dies includes shot peening the interior die cavity walls with substantially spherical shot having a hardness value at le...

  • Abrasives Distributor
  • Year: 1986, Source: US Patent 4,569,159
  • A novel abrasives distributor is disclosed. The distributor comprises a movable assembly, and at least one gun. The assembly preferably includes an elongated, hollow shaft having an inlet, and a hollo...

  • Tool and Method for Rotopeening the Peripheral Tubes in a Tubesheet
  • Year: 1986, Source: US Patent 4,713,952
  • An improved apparatus and process for rotopeening metallic conduits of limited accessibility, such as the peripherally located heat exchange tubes around the tubesheet of a nuclear steam generator, is...

  • Sensor for the Detection of Random Signals which are Suitable for Correlative Signal Processing
  • Year: 1986, Source: US Patent 4,604,904
  • The sensor is intended for the detection of random signals suitable for correlative signal processing, originating from a process in motion relative to the sensor for example a flow passing through a ...

  • System For The Monitoring And Control Of Flow Of Particulate Material In Impact Treatment Equipment
  • Year: 1986, Source: US Patent 4,614,100
  • Air blast peening equipment includes a flow density transducer and a pressure or velocity transducer for measuring flow velocity. Measured values are compared during peening with predetermined desire...

  • Peened Overlay Coatings
  • Year: 1985, Source: US Patent 4,514,469
  • Disclosed are coatings which are improved by a special peening process. Uniform sized spherical steel shot, in the range 1-2.5 mm is impacted at uniform low velocities onto a coated workpiece. Peening...


Previous     15   16   17   18   19   20   21   22   23       Next

The Shot Peener magazine

The Shot Peener magazine is dedicated to sharing information and expanding global markets for the shot peening and blast cleaning industries. We cover topics of importance to a wide range of readers -- from OEMs to engineers to academics to machine operators -- in a fresh and engaging format. The magazine is free of charge to make it accesssible to as large an audience as possible.

Electronics Inc. publishes the magazine. For more information, visit The Shot Peener magazine.

Sponsored by Electronics Inc. © 2026 Electronics Inc. All Rights Reserved.