  • Expanding the Parameters of Almen Strip Manufacturing
  • Year: 2013, Source: The Shot Peener magazine, Vol 27, Issue 2, Spring 2013
  • An Almen strip that meets specification parameters in flatness (prebow), hardness and thickness isn’t always good enough. The following is a real-life example of strips that met specs, but fail...

  • Advice for New Shot Peening Technicians
  • Year: 2013, Source: The Shot Peener magazine, Vol 27, Issue 2, Spring 2013
  • Elmer Smith, a Process Engineer with Spirit AeroSystems in Wichita, Kansas, exemplifies the best of the manufacturing workforce. He is an experienced technician that enjoys his job and does it well. H...

  • Strength in Numbers
  • Year: 2013, Source: The Shot Peener magazine, Vol 27, Issue 2, Spring 2013
  • Many years ago, when I joined the Aerospace Metals Engineering Committee (AMEC) of the Aerospace Materials Division of the Society of Automotive Engineers, I found that shot peening was scarcely ...

  • iBlue: The First Industrial Bluetooth Transmitter
  • Year: 2013, Source: The Shot Peener magazine, Vol 27, Issue 1, Winter 2013
  • ITAMCO (Indiana Technology and Manufacturing Companies)has released the iBlue—the first handheld bluetooth transmitter that gathers crucial production data and sends it to bluetooth-enabled sma...

  • Industry News
  • Year: 2013, Source: The Shot Peener magazine, Vol 27, Issue 1, Winter 2013
  • WG Plus De Mexico Celebrates Open House Joel McGreal, Promoted to General Sales Manager Asbury Wilkinson Joins Ervin Amasteel Shot and Grit and Amacast Cast Stainless Steel Shot....

  • Need Information? Join the Shot Peening Universe Forums
  • Year: 2013, Source: The Shot Peener magazine, Vol 27, Issue 1, Winter 2013
  • Do you have a question related to shot peening or blast cleaning? The Forum at www.shotpeener.com is a great place to post a question and get answers from industry experts around the world. The Forum ...

  • Principles of Almen Strip Selection
  • Year: 2013, Source: The Shot Peener magazine, Vol 27, Issue 1, Winter 2013
  • INTRODUCTION: The guiding principles for Almen strip selection are thickness, variability and shape. Thickness selection, N, A or C is a normally matter for users rather than shot peeners. Thickness ...

  • New Manufacturing Project to Save Millions in Reclaimed Parts
  • Year: 2013, Source: The Shot Peener magazine, Vol 27, Issue 1, Winter 2013
  • RECLAIM, a cutting-edge project at the £40 million Manufacturing Technology Centre (MTC) in Coventry, United Kingdom, has the potential to save UK industry millions of pounds by re-manufacturing...

  • Glass Bead Polishes Apple
  • Year: 2013, Source: The Shot Peener magazine, Vol 27, Issue 1, Winter 2013
  • Apple’s first flagship store in New York’s SOHO district brings to mind an Apple notebook: a spare, elegant metal housing for its ground-breaking technology. It was one of several Ap...

  • Hali Diep Named 2012 Shot Peener of the Year
  • Year: 2013, Source: The Shot Peener magazine, Vol 27, Issue 1, Winter 2013
  • The Shot Peener magazine has named Hali Diep as the 2012 Shot Peener of the Year. Mr. Diep is an Associate Technical Fellow in Surface Enhancement/Shot Peening at Boeing Research and Technology. He...

  • An Alternative Solution to Shot Peening Challenges
  • Year: 2013, Source: The Shot Peener magazine, Vol 27, Issue 1, Winter 2013
  • The Comco Journey Into Shot Peening Comco Inc., a California-based company, has 40 years of experience providing micro-abrasive blasting technology to medical, microelectronics, precision machining...

  • Change Is Inevitable, Growth Is an Option
  • Year: 2013, Source: The Shot Peener magazine, Vol 27, Issue 1, Winter 2013
  • We all like change—when someone else does the changing. We get the latest and greatest version of whatever product (read Toys for Boys). We don’t want last year’s car model or ...

  • J 443 An Evolutionary Guide to Shot Peening Intensity Measurement
  • Year: 2012, Source: The Shot Peener magazine, Vol 26 / Issue 2, Spring 2012
  • INTRODUCTION J443 – Procedures for Using Standard Shot-Peening Test Strip, was first approved in January, 1952. As an SAE Recommended Practice document the principles that it enshrined were wid...

  • Shooting at Ceramics
  • Year: 2012, Source: The Shot Peener magazine, Vol 26 / Issue 4, Fall 2012
  • RESEARCH REPORT: In corrosive, high-temperature environments, metals quickly lose their elasticity. Beyond certain temperatures the material fails and its properties are compromised; metallic spring...


Previous     35   36   37   38   39   40   41   42   43       Next

The Shot Peener magazine

The Shot Peener magazine is dedicated to sharing information and expanding global markets for the shot peening and blast cleaning industries. We cover topics of importance to a wide range of readers -- from OEMs to engineers to academics to machine operators -- in a fresh and engaging format. The magazine is free of charge to make it accesssible to as large an audience as possible.

Electronics Inc. publishes the magazine. For more information, visit The Shot Peener magazine.

Sponsored by Electronics Inc. © 2026 Electronics Inc. All Rights Reserved.