Accuracy of computerized saturation curve analysis
Author: Dr. David Kirk
Source: The Shot Peener magazine, Vol 20 / Issue 1, Winter 2006
Doc ID: 2006050
Year of Publication: 2006
Abstract:
INTRODUCTION Accuracy has two components: precision and bias. Attention has to be paid to both components if we are to achieve high levels of accuracy. Imagine that we have a digital thermometer, sensitive to changes of 0.001