Accurary of Declared Peening Intensity Values
Author: David Kirk, Hon Research Fellow, Coventry Univ
Source: The Shot Peener magazine, Vol 24 / Issue 2, Spring 2010
Doc ID: 2010011
Year of Publication: 2010
Abstract:
Academic Study by Dr. David Kirk
INTRODUCTION
Peening intensity is the arc height of one particular point on a simulated saturation curve that is declared as meeting specification requirements. Three stages are involved:
(i) Generation of a Data Set