SHOT PEENING AUTOMATION
Author: Anja Črtalič | Marketing Manager | FerroCrtalic International
Source: The Shot Peener magazine, Vol 36, Issue 3, Summer 2022
Doc ID: 2022031
Year of Publication: 2022
Abstract:
SHOT PEENING is a process that requires a high level
of control to achieve work process repeatability. The main
reason for that is one cannot check the peening effect on
actual material without destructive testing, so it is crucial to
control all parameters that affect intensity in order to ensure
that the shot peening process is done according to requirements.
Today’s machines are equipped with PLC and HMI
control; therefore, almost everything can be controlled and
stored in case reverse checking is needed. For controlling
their shot peening machines, FerroECOBlast uses their own
platform called FerroSmartPanel, which can be set up on any
HMI or PLC brand. It has been designed in-house based on
our extensive know-how and experience in surface treatment
gained since 1964.
| Download PDF |
|---|