  • Surface Treatment Device Including Magnetic Shot Separator
  • Year: 1978, Source: US Patent 4,080,760
  • A magnetic separator is disclosed suitable for incorporation in a surface teatment device, such as, a particulate throwing whel employing a rebound system to recycle the particulate. The separator in...

  • Method of Abrading or Having a Restricted Passage Surface
  • Year: 1978, Source: US Patent 4,087,943
  • A flowable abrasive composition comprising a poluboronorgano silicon compound and dispersed abrasive granules, said composition being modified with a gel formed from a metallic soap(8-22 carbon atoms)...

  • Sandblast Abrading Apparatus
  • Year: 1978, Source: US Patent 4,067,150
  • Air from a source of pressurized air, acting through a ball-type vibrator and a resilient mounting, serves to form a cloud of abrasive material within a reservoir of such material. Air from the same ...

  • Process Of Shot Peening And Cleaning And Preparing Shot Pellets Thereof
  • Year: 1978, Source: US Patent 4,067,240
  • A process of compression stressing shot pellets to increase the fatigue strength or resistance thereof to brittle fractures by impact of the pellets during shot peening and cleaning operations wherein...

  • Method And Apparatus For Measuring Intensity Of Peening Of Small Surfaces
  • Year: 1978, Source: US Patent 4,102,176
  • The peening intensity test member is a factory assembled unit comprising a base structure having opposite faces and a test element secured to one of the faces of the base structure, the test element b...

  • Apparatus for Producing Spherical Particles
  • Year: 1977, Source: US Patent 4,046,548
  • ABSTRACT A system for producing glass spheres in which the combustion air introduced into the furnace iw preheated. The furnace has a shroud enclosing at least a portion of its outer surface, and amb...

  • Glass Bead Forming Nozzles and Method
  • Year: 1977, Source: US Patent 4,002,447
  • ABSTRACT The diameters of glass beads formed by jetting molten glass through an orifice are changed without a shutdown by employing an orifice nozzle having a tapered tip. With such a nozzle, the bea...

  • Glass Bead Forming Method
  • Year: 1977, Source: US Patent 4,002,446
  • Spherical regularity of glass beads is improved by catching a falling stream of hot beads in a bath of liquid quenching medium having a relatively low heat transfer coefficient controlled by maintaini...

  • Descaling Bent Rod With Separated Cleaning Particles
  • Year: 1977, Source: US Patent 4,004,374
  • A method of descaling a rod comprises forming at least one bend in the rod and rotating the bent portion in an approximately circular path while maintaining it in a space having a distribution of sepa...

  • Vibratory Finishing Device
  • Year: 1977, Source: US Patent 4,018,009
  • A finishing device in the form of an annular bowl adapted to house media and parts to be finished and means for imparting vibratory energy to the bowl to cause the media and parts to progress in agita...

  • Surface Treatment Device for Large Diameter Pipe Sections
  • Year: 1977, Source: US Patent 4,016,681
  • A surface treatment device is disclosed which is capable of efecting surface treatment of the inside and outside of large diameter pipi sections. The device preferably employs an airless centrifugal b...

  • Conditioning Cleanser for Ceramic Surfaces
  • Year: 1977, Source: US Patent 4,035,163
  • An alkaline cleaning and conditioning composition for ceramic surfaces is provided in the form of an abrasive powder mixture including a surfactant, and a silicone oil absorbed in a water soluable obs...

  • Flow Control System
  • Year: 1977, Source: UK Patent 1,481,021
  • The present invention concerns control systems for controlling flowing materials and is particularly concerned with controlling the flow of particulate materials carried by a fluid medium. ...

  • Process Of Compression Stressing Metals To Increase The Fatigue Strength Thereof
  • Year: 1977, Source: US Patent 4,034,585
  • A process of compression stressing metals to increase the fatigue strength or resistance to brittle fractures thereof by shot peening or surface rolling wherein the elastic radial tensile stress of th...


Previous     20   21   22   23   24   25   26   27   28       Next

The Shot Peener magazine

The Shot Peener magazine is dedicated to sharing information and expanding global markets for the shot peening and blast cleaning industries. We cover topics of importance to a wide range of readers -- from OEMs to engineers to academics to machine operators -- in a fresh and engaging format. The magazine is free of charge to make it accesssible to as large an audience as possible.

Electronics Inc. publishes the magazine. For more information, visit The Shot Peener magazine.

Sponsored by Electronics Inc. © 2026 Electronics Inc. All Rights Reserved.