  • Centrifugal Blasting Wheel
  • Year: 1972, Source: US Patent 3,694,963
  • A centrifugal blasting wheel provided with throwing blades whose throwing surfaces are flat and parellel to the axis of rotation of the wheel at their inner ends and slope gradually so that their oute...

  • Improvements in or relating to the measurement of the flow of particulate material
  • Year: 1972, Source: UK Patent 1,270,112
  • The invention relates to the measurement of the flow of particlulate materials conveyed hydrodynamically by means of a flowing fluid and more particularly, but not exclusively, to the measurement of t...

  • Shot Peening Method
  • Year: 1972, Source: US Patent 3,705,510
  • Metal sheets are peen formed by projecting peening shot from centrifugal shot throwing wheels against the sheet passing thereunder. The centrifugal shot throwing wheels are also used for saturation p...

  • Method Of And Apparatus For Measuring Intensity Of Peening In Small Hole Diameter Holes
  • Year: 1972, Source: US Patent 3,695,091
  • The method of measuring intensity of peening in the Almen scale of small diameter holes, such as 0.5 inch or less, consists of a first step of plotting an intensity curve on a reference graph, which i...

  • Method Of After-treatment Of Metal Platings
  • Year: 1972, Source: US Patent 3,701,677
  • Metal articles plated with metals having a tendency of forming cracks in the deposited metals are subjected to a jet stream of solid particles such as glass beads to eliminate the cracks....

  • Metal Surface Treating Apparatus For Internal Surfaces
  • Year: 1972, Source: US Patent 3,654,786
  • The metal surface treating apparatus comprises a tubular lance, which is supported for rectilinear movement and connected to receive pressurized fluid and solid particles and discharge the same from o...

  • Low Penetration Ball Forming Process
  • Year: 1972, Source: US Patent 3,705,511
  • A controlled metal deformation process for shaping, forming or contouring metal sheet, plate, and wrought shapes such as extrusions comprising flowing a quantity of metal balls (generally greater in s...

  • Apparatus For Shot Peening Turbine Blades.................
  • Year: 1972, Source: US Patent 3,668.913
  • A turntable having a number of pairs of opposed resilient gripping members mounted on nested ring members, one of the rings having its axis eccentrically translatable relative to the other, the transl...

  • Adjustable Cyclone Separator
  • Year: 1972, Source: US Patent 3,667,196
  • In a cyclone separator, a valve means adjustable to cause partial by-pass of gaseous fluid and solid particles entrained therein from the separation chamber to the gaseous fluid outlet. Also, means i...

  • Apparatus for Filtering Suspended Soldis from Gaseous Medium and for Removal of Filter Cake from Filter Elements
  • Year: 1971, Source: US Patent 3,606,736
  • Apparatus for gaseous filtration to effect removal of suspended solids in which use is made of clongate filter elements having an open end and means for flowing gaseous medium containing the suspended...

  • Quick-Drying Scouring Composition
  • Year: 1971, Source: US Patent 3,607,161
  • A scouring composition comprising a cationic surface active compound and a water-soluable abrasive which leaves a surface which has been cleaned dry, shiny an dfree from gritty residue film....

  • Methods For Improving Hardness And Strength Of Ceramic Materials
  • Year: 1971, Source: US Patent 3,573,023
  • Methods for improving the hardness and strength of frangible or relatively brittle materials, involving surface deformation by mechanical means to establish compressive stresses in the material surfac...

  • Apparatus For Surface Treating Work Pieces
  • Year: 1971, Source: US Patent 3,566,644
  • The apparatus for the surface treating of work pieces comprises a motor and a centrifugal throwing wheel connected for rotation to the motor, the throwing wheel having an axially arranged feed inlet f...

  • Method and Apparatus for Manufacturing Small Beads by Centrifugal Action
  • Year: 1970, Source: US Patent 3,499,745
  • ABSTRACT OF THE DISCLOSURE A method and apparatus for producing tiny spherical beads by applying molten glass to at least one surface of a rotating centrigual member, permitting the molten glass to s...


Previous     23   24   25   26   27   28   29   30   31       Next

The Shot Peener magazine

The Shot Peener magazine is dedicated to sharing information and expanding global markets for the shot peening and blast cleaning industries. We cover topics of importance to a wide range of readers -- from OEMs to engineers to academics to machine operators -- in a fresh and engaging format. The magazine is free of charge to make it accesssible to as large an audience as possible.

Electronics Inc. publishes the magazine. For more information, visit The Shot Peener magazine.

Sponsored by Electronics Inc. © 2026 Electronics Inc. All Rights Reserved.