Patents Relating to Shot Peening

The articles below are archived in the shotpeener.com Library. You can search these articles by using the keyword search below. Click on an article title to view details and access a free full text pdf. Search Tips

Total articles (550)

Page 31 of 40

  • Refrigeration System for Cold Vapor Blast
  • Year: 1966, Source: US Patent 3,276,219
  • This invention relates to a system for the refrigerationof parts by means of a stream of cold air or other gas or fluid and it relates more particularly to a system of the type described having a flex...

  • Machine for Controlled Freezing, Deflashing and trimming of Parts
  • Year: 1966, Source: US Patent 3,279,125
  • This inventin relates to the removal of thin fins, furrs and flashings from parts molded of rubber, plastics, metal and the like materials which are capable of embrittlement or are changed in physical...

  • Stress Peening Steel Articles
  • Year: 1966, Source: US Patent 3,438,229
  • Apparatus and process for stress peening steel articles such as automobile leaf springs wherein a spring is deflected from a free configuration to a contour corresponding to that condition of the spri...

  • Process For Surface Altering
  • Year: 1966, Source: US Patent 3,257,759
  • This invention relates to a process for hydraulic blasting and surface-altering of articles. The invention utilizes hydraulic means for imparting energy to surface-altering particles, such as so-call...

  • Method And Means For Continuous Surface Treatment
  • Year: 1966, Source: US Patent 3,5l7,465
  • A means and method for surface treatment of shaped articles of large dimension by throwing particulate material onto the surfaces of the articles, an open cage having circular rims into which the arti...

  • Metal Shot Producing Apparatus
  • Year: 1966, Source: US Patent 3,271,992
  • This invention concerns an apparatus for increasing the yield of fine metal shot from a single heat of metal and a machine for converting metal grit to shot for use therein. In its broadest sense, t...

  • Magnetic Wear Plates For Abrasive Blasting Chambers
  • Year: 1966, Source: US Patent 3,242,616
  • The present invention relates to abrasive blasting chambers having their inner surfaces protected with magnetic wear plates....

  • Abrasive Blasting Apparatus
  • Year: 1966, Source: US Patent 3,270,464
  • This invention relates to abrasive blasting apparatus for machining work pieces, particularly, silicon wafers. Silicon wafers used in the electronics industry must be made with precise dimensions. ...

  • Scaling Tool
  • Year: 1965, Source: US Patent 3,343,246
  • A scaling tool driven by a rotating electric motor having a cam drive arrangement which converts rotary to reciprocating motion driving a needle scaling head together with a bundle of needles therein ...

  • Means for Treating Coil Springs
  • Year: 1965, Source: US Patent 3,383,803
  • A machine for surface treatment of continuous pitch coil springs comprising horizontally disposed roll cluster having a feed end at one end portion and a delivery end at the opposite end portion and i...

  • Adapter for Reciprocating Hammer
  • Year: 1965, Source: US Patent 3,359,611
  • A scaling tool having a plurality of active elements or needles for removing paint and rust from a steel surface adapted for connection with a conventional reciprocating air or electric hammer for lon...

  • Method for Increasing Endurance Limit of Steel Articles
  • Year: 1965, Source: US Patent 3,205,556
  • This invention relates, as indicated, to a method for improving certain characteristics of steel articles, and more particularly to a method for increasing the strength and hardness characteristics of...

  • Surface Treatment Of Steel
  • Year: 1965, Source: US Patent 3,188,776
  • This invention relates to a process for the surface treatment of steel and, in particular, to the treatment of hot worked steel having mill scale thereon....

  • Forming Round Balls
  • Year: 1965, Source: US Patent 3,204,320
  • This invention relates in general to an economical method and apparatus for mechanically producing small, substantially spherical balls from non-spherical metal blanks....


Previous     27   28   29   30   31   32   33   34   35       Next

The Shot Peener magazine

The Shot Peener magazine is dedicated to sharing information and expanding global markets for the shot peening and blast cleaning industries. We cover topics of importance to a wide range of readers -- from OEMs to engineers to academics to machine operators -- in a fresh and engaging format. The magazine is free of charge to make it accesssible to as large an audience as possible.

Electronics Inc. publishes the magazine. For more information, visit The Shot Peener magazine.

Sponsored by Electronics Inc. © 2026 Electronics Inc. All Rights Reserved.