  • Fluorescent Penetrant Inspection Materials And Methods
  • Year: 1960, Source: US Patent 2,920,203
  • This invention relates to improvements in materials and methods for the non-destructive testing of materials, pieces, parts, or structures (also hereinafter referred to as "test bodies") for subsurfac...

  • Centrifugal-type Fluid Purifier
  • Year: 1960, Source: US Patent 2,952,330
  • The present invention provides several novel features in the art of centrifuges. For one thing, the only motion within the device is that of the fluid itself passing through the purifier in two or mo...

  • Polishing Method and Device
  • Year: 1959, Source: US Patent 3,090,166
  • This invention relates to the art of polishing or surface finishing and it relates more particularly to a method and means for polishing the surfaces of metal and the like materials in a low cost, con...

  • Separator for Particulate Materials
  • Year: 1959, Source: US Patent 3,005,547
  • This invention relates to an improved device for separating particulate materails, such as dust from abrasive granules; and more particurly to an improved device for abstracting fine contaminants from...

  • Shot Peening Apparatus
  • Year: 1959, Source: US Patent 2,900,765
  • This invention pertains to centrifugal blasting apparatus, and particularly to a centrifugal propelling machine for selective shot peening. The present invention relates to apparatus for automatical...

  • Shot Peening Apparatus
  • Year: 1959, Source: US Patent 2,881,506
  • This invention relates generally to shot peening apparatus of the type in which small shot particles are forcibly impacted against surfaces of parts for cold working purposes, and more particularly ha...

  • Continuous Method For Conditioning Wire
  • Year: 1959, Source: US Patent 2,913,354
  • This present invention relates to a method and apparatus for making rods in a continuous operation. More particularly, this invention relates to a method and apparatus for continuous manufacture of...

  • Chromium Bearing Surface
  • Year: 1958, Source: US Patent 3,063,763
  • The present invention relates to chrmium bearing surfaces for cylinder liners, cylinder bores, shafts or the like. It relates, more particularly, to chromium bearing surfaces of a type which contains ...

  • Reformation of Metallic Surfaces
  • Year: 1958, Source: US Patent 3,019,522
  • This invention relates generally to the reformation of metallic surfaces presenting substantially contguous, relatively sharp microscopic crests, points or ridges, and depressions, or valleys, which m...

  • Panel Forming Equipment
  • Year: 1958, Source: US Patent 3,004,584
  • This invention relates generally to methods and apparatus for forming panels into desired spatial configuration, and more particularly has to do with economically forming long panels and tapered panel...

  • Valve Mechanisms For Magnetic Fluid Conduits And Devices Employing The Same
  • Year: 1958, Source: US Patent 2,820,471
  • The present invention relates to valve mechanisms for magnetic fluid conduits and to uses thereof, for example, shock absorbers. The general object of the present invention is to provide such valve...

  • Centrifugal Blasting Wheel And Blades For Use In Same
  • Year: 1958, Source: US Patent 2,819,562
  • This invention relates to wheels for throwing abrasive particles centrifugally at high velocity against surfaces to be cleaned or otherwise treated and it relates more particularly to blades for use i...

  • Flowmeter
  • Year: 1957, Source: US Patent 2,781,660
  • The present invention relates to flowmeters, especially suited for the measurement of flow in liquids which are opaque, and particularly for measuring the extracorporeal flow of animal (including huma...

  • Producing Metal Balls By Propelling Against An Anvil
  • Year: 1956, Source: US Patent 2,758,360
  • This invention relates to the production of steel shot or balls especially to small steel balls for use as shot in ammunition or shot gun shells and the like, or else for use as ball bearings, or for ...


Previous     30   31   32   33   34   35   36   37   38       Next

The Shot Peener magazine

The Shot Peener magazine is dedicated to sharing information and expanding global markets for the shot peening and blast cleaning industries. We cover topics of importance to a wide range of readers -- from OEMs to engineers to academics to machine operators -- in a fresh and engaging format. The magazine is free of charge to make it accesssible to as large an audience as possible.

Electronics Inc. publishes the magazine. For more information, visit The Shot Peener magazine.

Sponsored by Electronics Inc. © 2026 Electronics Inc. All Rights Reserved.