  • Peening Nozzle
  • Year: 1968, Source: US Patent 3,419,894
  • This disclosure is directed to a nozzle for ejecting shot at high velocity for peening operations. The nozzle is fed from a hopper with the input peening shot being all supplied under a like head. T...

  • Flow Regulation Valve For Magnetic Particles
  • Year: 1968, Source: US Patent 3,406,704
  • A valve for regulating the flow of materials which are made up of a substantial portion of magnetic particles. The valve includes an outer member and an assembly consisting of a permanent magnet and ...

  • Improved Method of and Equipment for Shot-blasting and the Like
  • Year: 1967, Source: British Patent 1,084,496
  • ..........this invention is based on the fact that a particle of ferromagnetic material introduced into a magnetic field tends to be drawn towards the region of highest energy density. The invention m...

  • Dry-Lubricated Surface and Method of Producing such Surfaces
  • Year: 1967, Source: US Patent 3,574,658
  • Dry lubricant such as molybdenum disulfide is applied to a solid surface by interposing the lubricant between the surface and a force generating means such as a peeining particle, preferably by applyi...

  • Apparatus for Ornamenting Articles
  • Year: 1967, Source: US Patent 3,520,086
  • Apparatus for mass producing engraved glass articles comprises a pluralit of spaced apart abrasive blasting stations and a main conveyor for moving the glass articles through each of said stations at ...

  • Power Tool Adjustment Device
  • Year: 1967, Source: US Patent 3,451,490
  • A power tool attachment which controls the depth of penetration or exposure of the power instrument, such as a drill or the like. Two concentric cylinders having coincident longitudinal slots are fitt...

  • Adjustable Peening Tool
  • Year: 1967, Source: US Patent 3,444,714
  • The disclosure pertains to a tool having a rotatable cage with tapered rollers supported therin and engaged by a central tapered end of a driving arbor. The tapered end had axially disposed flutes the...

  • Workpiece Treating Apparatus
  • Year: 1967, Source: US Patent 3,521,406
  • A workpiece treating apparatus includes a throwing wheel which is universally mounted for rotation about a plurality perpendicular axes. Additionally, the wheel is mounted for movement in the vertica...

  • Particle-Throwing Apparatus
  • Year: 1967, Source: US Patent 3,319,383
  • The present invention relates to particle-throwing apparatus, more particularly to apparatus of the type shown in U.S. Patent 2,732,666, granted Jan. 31, 1956. Such apparatus includes a wheel that ro...

  • Method Of Producing Propping Agent
  • Year: 1967, Source: US Patent 3,316,748
  • This invention relates to system for increasing the yield of underground formations such as oil wells. More particularly, this invention concerns aluminum particles of appropriate size and strength t...

  • Controlled Glass Bead Peening
  • Year: 1967, Source: US Patent 3,531,964
  • A method and apparatus for inducing compressive stresses in a pressure vessel to prevent stress corrosion. The apparatus consists of mechanism for rotating the pressure vessel while a lance carrying ...

  • Method and Apparatus for Manufacturing Glass Beads
  • Year: 1966, Source: US Patent 3,293,014
  • The present invention relates to the production of glass beads and more particularly to a method of producing glass beads directly from a molten stream of glass, but is in no way limited thereto....

  • Descaling Tool
  • Year: 1966, Source: US Patent 3,349,461
  • A needle-type descaling tool which includes a fluid motor casing and a tubular sleeve removably attached to the casing. A needle holder is mounted in the forward end of the tubular sleeve. There is an...

  • Continuous Cleaning Apparatus
  • Year: 1966, Source: US Patent 3,903,652
  • Automotive heads and manifolds or like molded or cast articles are continuously cleaned by projected streams of impinging particles, by pushing a series of such articles axially into one end of an elo...


Previous     26   27   28   29   30   31   32   33   34       Next

The Shot Peener magazine

The Shot Peener magazine is dedicated to sharing information and expanding global markets for the shot peening and blast cleaning industries. We cover topics of importance to a wide range of readers -- from OEMs to engineers to academics to machine operators -- in a fresh and engaging format. The magazine is free of charge to make it accesssible to as large an audience as possible.

Electronics Inc. publishes the magazine. For more information, visit The Shot Peener magazine.

Sponsored by Electronics Inc. © 2026 Electronics Inc. All Rights Reserved.