  • Centrifugal Blasting Apparatus
  • Year: 1956, Source: US Patent 2,732,666
  • The present invention relates to centrifugal blasting apparatus, more particularly to such apparatus as that shown in U.S. Patent No. 2,582,702, granted January 15, 1952, which apparatus projects a di...

  • Blast Gun
  • Year: 1956, Source: US Patent 2,751,716
  • This invention relates to improvements in sand blasting guns of the type using a high pressure of water for scouring or cleaning work or surfaces, the water being mixed with air or sand and detergents...

  • Method of Strengthening and Repairing Damaged Threads
  • Year: 1955, Source: Canadian Patent 2 538 509
  • A method of strengthening and repairing damaged threads. Firstly, remove metal buildup from the damaged threads. Secondly, peen the damaged threads using glass beads. The glass beads are not less than...

  • Separators for Pneumatically Conveyed Aggregate Goods
  • Year: 1955, Source: US Patent 2,850,162
  • This invention relates to separators, and more particularly to separators for pneumatically conveyed aggregate goods wherein the goods are cleaned and sorted by the conveying medium....

  • Method Of Cold Forming Sheets
  • Year: 1955, Source: US Patent 2,701,408
  • This invention relates to the art of metal forming and relates more particularly to methods and apparatus for shaping or forming metal sheets and plates. While the invention has a wide range ...

  • Device For Separating Mixed Masses Of Spher.and Irreg.shaped Bodies Such As Seeds,grains And The Lik
  • Year: 1955, Source: US Patent 2,724,498
  • This invention relates to an improved type of gravity feeding device for selectively separating a mixed mass of irregularly shaped and spherically shaped bodies from each other. More specifically, it...

  • Centrifugal Blasting Wheel
  • Year: 1955, Source: US Patent 2,708,814
  • This invention relates to a centrifugal blasting machine and more particularly to a device for accelerating the movement of particulate substances, such as metallic shot or grit, sand and similar non-...

  • Apparatus For Descaling And Coating Wire
  • Year: 1955, Source: US Patent 2,703,550
  • The present invention relates to a method of and apparatus for removing scale deposits from elongated metal articles such as wire, rods, sheets and the like....

  • Method of Forming Malleableized Iron Castings
  • Year: 1954, Source: US Patent 2,796,373
  • The present invention broadly relates to the art of metal treatment. The invention particularly relates to a method of producing ferrous castings and the casting so produced. This application is a c...

  • Magnetic Valve
  • Year: 1954, Source: US Patent 2,670,749
  • This invention relates to valves for controlling the flow of fluids and has for a general object the provision of a new and improved means and method for controlling the flow of fluids by a magnetic f...

  • Tools for Roughening Surfaces
  • Year: 1953, Source: US Patent 2,799,035
  • My invention relates to tools for roughening surfaces, and is particularly adapted for roughening surfaces on what it is desired to bind a filling material, such as in dents in automobile bodies and t...

  • Field Sensitive Hydraulic Apparatus
  • Year: 1953, Source: US Patent 2,651,258
  • This invention relates to hydraulic apparatus, and more particularly to hydraulic apparatus and systems employing a fluid which is sensitive to fields such as an electro-magnetic field....

  • Shot Peening Test Fixture
  • Year: 1952, Source: US Patent 2,607,213
  • This invention relates generally to the shot peening of axle shafts and more specifically to a fixture for holding test strips for measuring the intensity of the shot peening....

  • Method Of Sandblasting
  • Year: 1952, Source: US Patent 2,617,225
  • This invention relates to sandblast stencils, and more particularly to those employing a composition including rubber and used for the ornamenting, cutting or carving of stone by a sandblasting proces...


Previous     31   32   33   34   35   36   37   38   39       Next

The Shot Peener magazine

The Shot Peener magazine is dedicated to sharing information and expanding global markets for the shot peening and blast cleaning industries. We cover topics of importance to a wide range of readers -- from OEMs to engineers to academics to machine operators -- in a fresh and engaging format. The magazine is free of charge to make it accesssible to as large an audience as possible.

Electronics Inc. publishes the magazine. For more information, visit The Shot Peener magazine.

Sponsored by Electronics Inc. © 2026 Electronics Inc. All Rights Reserved.