Articles from The Shot Peener magazine

The articles below are archived in the shotpeener.com Library. Click on an article title below to view details and access a free full text pdf. Visit The Shot Peener magazine website for more information about the magazine and to download complete issues.

Total articles (1210)

Page 50 of 87

  • Generic Almen Fixtures for Intensity Measurement in Shot Peening
  • Year: 2008, Source: The Shot Peener magazine, Vol 22 / Issue 1, Winter 2008
  • Applying the shot peening process on aerospace parts can be a tough challenge as geometries can get complicated and requirements quite strict. Documented cases of aerospace component failures also rem...

  • Shot Peening of Springs-a Case Study
  • Year: 2008, Source: The Shot Peener magazine, Vol 22 / Issue 1, Winter 2008
  • Acknowledgments: The investigation that formed the basis for this article was instigated by the author in cooperation with four organizations that participated in experimental efforts as follows: the ...

  • Putting Turbulence to Work
  • Year: 2008, Source: The Shot Peener magazine, Vol 22 / Issue 1, Winter 2008
  • Here's one of those wish-I'd-thought-of-it-first products that turns a liability into an asset. Steven Carpenter, an engineer with extensive experience in the foundry industry and an owner and partner...

  • Generation of Wheel-Blast Shot Velocity
  • Year: 2007, Source: The Shot Peener magazine, Volume 21 / Issue 2, Spring 2007
  • INTRODUCTION Shot velocity is of primary importance because it governs the kinetic energy of the impacting shot and hence the peening intensity. Wheel-blast shot acceleration is much more energy-effic...

  • Generation of Air-Blast Shot Velocity
  • Year: 2007, Source: The Shot Peener magazine, Vol 21 / Issue 1, Winter 2007
  • Introduction Air-blast shot peening is well-established as the principal technique employed for precision peening. Shot particles are accelerated by a stream of compressed air fed into a nozzle. The m...

  • Crossing the Bridge
  • Year: 2007, Source: The Shot Peener magazine, Vol 21 / Issue 4, Fall 2007
  • We have a saying in America, "We will cross that bridge when we get to it." It means that we will delay dealing with a problem until we can no longer avoid it. That time is now for our overworked and ...

  • Planning, Communication and Documentation Lead to a Successful Purchase
  • Year: 2007, Source: The Shot Peener magazine, Vol 21 / Issue 4, Fall 2007
  • The two lists I've offered are intended to encourage the free flow of information between the customer and the equipment supplier. Each bit of information represents a springboard for development of a...

  • Modern Shot Blast Solutions for the Automobile Industry
  • Year: 2007, Source: The Shot Peener magazine, Vol 21 / Issue 4, Fall 2007
  • New concept for adapting manufacturing processes to a changing market environment Two of the most important issues currently facing the automotive industry are: - Reduction of vehicle weight for b...

  • Review of Shot Peened Surface Properties
  • Year: 2007, Source: The Shot Peener magazine, Vol 21 / Issue 4, Fall 2007
  • DISCUSSION AND CONCLUSIONS This account has, of necessity, involved broad generalisations about the properties of shot peened surfaces. That is because component materials vary enormously in terms of...

  • Hybrid Cleaning / Peening Machines
  • Year: 2007, Source: The Shot Peener magazine, Vol 21 / Issue 4, Fall 2007
  • Where do we go from here? With cost pressures from offshore manufacturing, it is time to tap into our history of innovative production skills. Our manufacturing has to get leaner and higher in produc...

  • Aerospace Engineering Degree Program Soars
  • Year: 2007, Source: The Shot Peener magazine, Vol 21 / Issue 4, Fall 2007
  • Nanyang Technological University (NTU) has successfully launched the first aerospace engineering degree program in Singapore. Singapore is positioned to become a global aerospace hub and Singapore'...

  • Extending the Fatigue Life of Bridges Using Stressonic Needle Peening
  • Year: 2007, Source: The Shot Peener magazine, Vol 21 / Issue 4, Fall 2007
  • CONCLUSION Stressonic needle peening is a great technique to re-establish or extend the life of bridges and other welded structures. The best and most cost-effective approach is to needle peen the we...

  • Effect of Shot Peening on Fatigue Behavior of 7055-T77 Aluminum alloy
  • Year: 2007, Source: The Shot Peener magazine, Vol 21/ No 4 Fall 2007 - From the Industry News section on page 35.
  • The effect of shot peening on 7055-T77 aluminum alloy has been investigated. 7055-T77 is a high strength alloy with microstructure of coarse grains and a pronounced metallurgical texture, both resulti...

  • The Parting Shot . . . Shot peening keeps pace with technology
  • Year: 2007, Source: The Shot Peener magazine, Volume 21 / Issue 3, Summer 2007
  • The Boeing Company is unveiling its long-awaited 787 Dreamliner this summer. It will be the first jet in 13 years from the commercial jet world leader that introduced the 707 in 1954. The company is b...


Previous     46   47   48   49   50   51   52   53   54       Next

The Shot Peener magazine

The Shot Peener magazine is dedicated to sharing information and expanding global markets for the shot peening and blast cleaning industries. We cover topics of importance to a wide range of readers -- from OEMs to engineers to academics to machine operators -- in a fresh and engaging format. The magazine is free of charge to make it accesssible to as large an audience as possible.

Electronics Inc. publishes the magazine. For more information, visit The Shot Peener magazine.

Sponsored by Electronics Inc. © 2026 Electronics Inc. All Rights Reserved.