EI Shot Peening Training and Syntech Surface Finishing Specialists will be co-hosting a shot peening seminar in Auckland, New Zealand, October 25-26.
The two-day training seminar is based on SAE specifications and it will cover all aspects of the shot peening process, including techniques and applications. Professional instructors will review how and why shot peening works, how to do it correctly, and how to inspect the completed process.
The following is a partial list of training topics:
- Shot Peening Introduction
- Understanding Intensity
- Process Inspection Equipment
- Generating Saturation Curves
- Saturation Curve Solving
- Parameter Adjustments
- Media Specifications and Inspection
- Peening Media Selection
- Maintaining Media Quality
- Peening Applications
- Peening Coverage
- Masking Options
- Lean Peening
- Surface Texture
- Peening Machine Design and Maintenance
- Understanding Residual stress Curves
- Advanced Processes
- Rotary-Flap Peening
The seminar fee is $1250 NZD per person and it includes tuition for both days of the seminar, a workbook, break refreshments, and lunch. The seminar will be held at the Grand Mercure Auckland.
Visit www.shotpeeningtraining.com to learn more and to register. Space is limited so register as soon as possible.